Fe-Cr合金气泡演化动力学的相场法模拟 |
| 刘彩艳, 冯泽华, 张云鹏, 余康, 吴璐, 马聪, 张静 |
|
Phase Field Simulation of Bubble Evolution Dynamics in Fe-Cr Alloys |
| LIU Caiyan, FENG Zehua, ZHANG Yunpeng, YU Kang, WU Lu, MA Cong, ZHANG Jing |
| 图3 不同Cr含量合金中气泡的演化过程 |
| Fig.3 Evolutions of bubbles in Fe-0Cr (a1-a5), Fe-3Cr (b1-b5), Fe-7Cr (c1-c5), Fe-11Cr (d1-d5), and Fe-13Cr (e1-e5) alloys at 1400t0 (a1-e1), 1600t0 (a2-e2), 2000t0 (a3-e3), 5000t0 (a4-e4), and 10000t0 (a5-e5) |
|