3D相场模拟研究Ti-6Al-4V合金片层组织形貌的影响因素 |
| 张瑶, 齐敏, 孙佳, 吴婷, 马英杰, 王皞, 杨锐 |
|
3D Phase Field Simulation of Factors Influencing the Microstructure Morphology of Lamellar Ti-6Al-4V Alloy |
| ZHANG Yao, QI Min, SUN Jia, WU Ting, MA Yingjie, WANG Hao, YANG Rui |
| 图10 820℃生长100 s时不同界面能各向异性条件下Al的溶质分布 |