3D相场模拟研究Ti-6Al-4V合金片层组织形貌的影响因素 |
| 张瑶, 齐敏, 孙佳, 吴婷, 马英杰, 王皞, 杨锐 |
|
3D Phase Field Simulation of Factors Influencing the Microstructure Morphology of Lamellar Ti-6Al-4V Alloy |
| ZHANG Yao, QI Min, SUN Jia, WU Ting, MA Yingjie, WANG Hao, YANG Rui |
| 图9 t = 1000 s时,kx 分别为0.4、0.6和0.8条件下晶粒不同x-z切面上片层的生长形貌 |
| Fig.9 Growth morphologies of lamellae on different x-z sections of grains under kxconditions of 0.4 (a1-c1), 0.6 (a2-c2), and 0.8 (a3-c3), respectively at t = 1000 s (a1-a3) x = 255.8Δx (b1-b3) x = 128.5Δx (c1-c3) x = 1.2Δx |
|