3D相场模拟研究Ti-6Al-4V合金片层组织形貌的影响因素 |
| 张瑶, 齐敏, 孙佳, 吴婷, 马英杰, 王皞, 杨锐 |
|
3D Phase Field Simulation of Factors Influencing the Microstructure Morphology of Lamellar Ti-6Al-4V Alloy |
| ZHANG Yao, QI Min, SUN Jia, WU Ting, MA Yingjie, WANG Hao, YANG Rui |
| 图4 晶粒不同z-x切面处侧枝在t = 2000 s的形貌(单元长度Δx = 5 × 10-8 m) |
| Fig.4 Morphologies of α side branches at different z-x sections at t = 2000 s (Unit length Δx = 5 × 10-8 m; the angle involved in the figure is the angle between the main layer and the side branches; Figs.4a-c are equivalent to Figs.4a1-c1, respectively) (a, a1) y = 23.85Δx (b, b1) y = 128.5Δx (c, c1) y = 252.85Δx (d) 2D slice layer α morphology[ |
|