镍基高温合金中S元素对基体与热障涂层界面稳定性的影响 |
| 王京京, 姚志浩, 张鹏, 赵杰, 张迈, 王蕾, 董建新, 陈迎 |
|
Effect of Element S on Interfacial Stability of Matrix and Thermal Barrier Coating in Nickle-Based Superalloys |
| WANG Jingjing, YAO Zhihao, ZHANG Peng, ZHAO Jie, ZHANG Mai, WANG Lei, DONG Jianxin, CHEN Ying |
| 图17 Ni3Al/NiAl体系(010)截面的电子局域化函数(ELF)投影图 |
| Fig.17 Electron localization function (ELF) projection in (010) plane of Ni3Al/NiAl system (a) clean (b) within S element |
|