镍基高温合金中S元素对基体与热障涂层界面稳定性的影响 |
| 王京京, 姚志浩, 张鹏, 赵杰, 张迈, 王蕾, 董建新, 陈迎 |
|
Effect of Element S on Interfacial Stability of Matrix and Thermal Barrier Coating in Nickle-Based Superalloys |
| WANG Jingjing, YAO Zhihao, ZHANG Peng, ZHAO Jie, ZHANG Mai, WANG Lei, DONG Jianxin, CHEN Ying |
| 图12 NiAl/Al2O3界面处S原子附近(010)面电荷密度分布 |
| Fig.12 Distribution of (010) surface charge density near S atom at NiAl/Al2O3 interface |
|