镍基高温合金中S元素对基体与热障涂层界面稳定性的影响 |
| 王京京, 姚志浩, 张鹏, 赵杰, 张迈, 王蕾, 董建新, 陈迎 |
|
Effect of Element S on Interfacial Stability of Matrix and Thermal Barrier Coating in Nickle-Based Superalloys |
| WANG Jingjing, YAO Zhihao, ZHANG Peng, ZHAO Jie, ZHANG Mai, WANG Lei, DONG Jianxin, CHEN Ying |
| 图10 Ni3Al/NiAl界面处S原子附近(010)面电荷密度分布 |
| Fig.10 Distribution of (010) surface charge density near S atom at Ni3Al/NiAl interface (The blue area in the legend represents negative values, indicating the charge decrease, while the green to red area represents positive values, indicating the charge increase. The same in Figs.12, 17, and 18) |
|