镍基高温合金中S元素对基体与热障涂层界面稳定性的影响 |
| 王京京, 姚志浩, 张鹏, 赵杰, 张迈, 王蕾, 董建新, 陈迎 |
|
Effect of Element S on Interfacial Stability of Matrix and Thermal Barrier Coating in Nickle-Based Superalloys |
| WANG Jingjing, YAO Zhihao, ZHANG Peng, ZHAO Jie, ZHANG Mai, WANG Lei, DONG Jianxin, CHEN Ying |
| 图3 Ni3Al(111)、NiAl(110)和Al2O3(0001)表面模型 |
| Fig.3 Surface models of Ni3Al(111) (a), NiAl(110) (b), and Al2O3(0001) (c) |
|