Cu-Co系难混溶合金核壳结构演化过程模拟 |
| 王霖, 魏晨, 王雷, 王军, 李金山 |
|
Simulation of Core-Shell Structure Evolution of Cu-Co Immiscible Alloys |
| WANG Lin, WEI Chen, WANG Lei, WANG Jun, LI Jinshan |
| 图7 Cu50Co50合金液相分离演变过程的模拟微观组织 |
| Fig.7 Simulated microstructures of Cu50Co50 alloy during liquid phase separation (a) t = 0.001 s (b) t = 0.004 s (c) t = 0.02 s (d) t = 0.04 s (e) t = 0.14 s (f) t = 0.2 s |
|