Cu-Co系难混溶合金核壳结构演化过程模拟 |
| 王霖, 魏晨, 王雷, 王军, 李金山 |
|
Simulation of Core-Shell Structure Evolution of Cu-Co Immiscible Alloys |
| WANG Lin, WEI Chen, WANG Lei, WANG Jun, LI Jinshan |
| 图4 第二相的凝并过程——显示了凝并过程中不同时刻下液桥的形成与演化 |
| Fig.4 Condensation process of the second phase showing the formation and evolution of the liquid bridge at different time during the condensation process (a) t = 0.002 s (b) t = 0.015 s (c) t = 0.02 s (d) t = 0.035 s (e) t = 0.1 s (f) t = 0.56 s |
|