316L不锈钢表面激光熔化沉积CoCrNiCu中熵合金的界面相容性 |
| 于云鹤, 谢勇, 陈鹏, 董浩凯, 侯纪新, 夏志新 |
|
Interfacial Compatibility for Laser Melting Deposition of CoCrNiCu Medium-Entropy Alloy on 316L Austenitic Stainless Steel Surface |
| YU Yunhe, XIE Yong, CHEN Peng, DONG Haokai, HOU Jixin, XIA Zhixin |
| 图12 316L不锈钢马氏体转变组织的透射Kikuchi衍射(TKD)分析 |
| Fig.12 Transmission Kikuchi diffraction (TKD) analyses of martensitic transformation microstructure in 316L stainless steel (a) SEM-SE image (b) PD figure (c) IPF (d-f) Kikuchi band patterns of positions 1 (d), 2 (e), and 3 (f) in Fig.12a |
|