316L不锈钢表面激光熔化沉积CoCrNiCu中熵合金的界面相容性 |
| 于云鹤, 谢勇, 陈鹏, 董浩凯, 侯纪新, 夏志新 |
|
Interfacial Compatibility for Laser Melting Deposition of CoCrNiCu Medium-Entropy Alloy on 316L Austenitic Stainless Steel Surface |
| YU Yunhe, XIE Yong, CHEN Peng, DONG Haokai, HOU Jixin, XIA Zhixin |
| 图7 CoCrNiCu MEA/316L不锈钢异种材料的固溶体判据计算结果 |
| Fig.7 Calculation results of solid solution criterions for the dissimilar materials of CoCrNiCu MEA and 316L stainless steel (a) Ω-δ criterion (Ω—ratio parameter, δ—atomic size difference) (b) mixing enthalpy (ΔHmix) criterion |
|