316L不锈钢表面激光熔化沉积CoCrNiCu中熵合金的界面相容性 |
| 于云鹤, 谢勇, 陈鹏, 董浩凯, 侯纪新, 夏志新 |
|
Interfacial Compatibility for Laser Melting Deposition of CoCrNiCu Medium-Entropy Alloy on 316L Austenitic Stainless Steel Surface |
| YU Yunhe, XIE Yong, CHEN Peng, DONG Haokai, HOU Jixin, XIA Zhixin |
| 图1 异种材料激光熔化沉积加工示意图和样品宏观形貌 |
| Fig.1 Schematic of laser melting deposition for dissimilar materials (a) and specimen macroscopic morphology of deposition layers with total scanning length of 18 cm (b) (MEA—medium-entropy alloy) |
|