Si对一种9Cr铁素体/马氏体钢显微组织和力学性能的影响 |
| 张乾坤, 胡小锋, 姜海昌, 戎利建 |
|
Effect of Si on Microstructure and Mechanical Properties of a 9Cr Ferritic/Martensitic Steel |
| ZHANG Qiankun, HU Xiaofeng, JIANG Haichang, RONG Lijian |
| 图8 P91和H-Si合金钢相转变温度的变化 |
| Fig.8 Changes of phase transition temperature of P91 and H-Si alloy steels |
|