电子束熔炼功率对GH4068合金微观组织、偏析和 γ′相析出行为的影响
白如圣, 谭毅, 崔弘阳, 宁莉丹, 崔传勇, 王云鹏, 李鹏廷

Effect of Electron Beam Smelting Power on Microstructure, Segregation, and γ′ Phase Precipitation Behavior of GH4068 Alloy
BAI Rusheng, TAN Yi, CUI Hongyang, NING Lidan, CUI Chuanyong, WANG Yunpeng, LI Pengting
图8 过热温度、形核过冷度与团簇结构变化的关系示意图
Fig.8 Schematic of relationships between superheat temperature, nucleation subcooling, and cluster structure change