Cu含量对K4061合金显微组织和拉伸性能的影响 |
| 曹姝婷, 赵剑, 巩桐兆, 张少华, 张健 |
|
Effects of Cu Content on the Microstructure and Tensile Property of K4061 Alloy |
| CAO Shuting, ZHAO Jian, GONG Tongzhao, ZHANG Shaohua, ZHANG Jian |
| 图11 K4061-10Cu合金热处理试样的TEM像和EDS元素线扫描图 |
| Fig.11 TEM image and EDS line scanning results of the K4061-10Cu alloy after heat treatment |
|