Cu含量对K4061合金显微组织和拉伸性能的影响 |
| 曹姝婷, 赵剑, 巩桐兆, 张少华, 张健 |
|
Effects of Cu Content on the Microstructure and Tensile Property of K4061 Alloy |
| CAO Shuting, ZHAO Jian, GONG Tongzhao, ZHANG Shaohua, ZHANG Jian |
| 图8 铸态K4061-8Cu和K4061-10Cu合金试样的SEM像和EDS元素面扫描图 |
| Fig.8 SEM images and corresponding EDS element maps of as-cast K4061-8Cu (a) and K4061-10Cu (b) alloys |
|