Cu含量对K4061合金显微组织和拉伸性能的影响 |
| 曹姝婷, 赵剑, 巩桐兆, 张少华, 张健 |
|
Effects of Cu Content on the Microstructure and Tensile Property of K4061 Alloy |
| CAO Shuting, ZHAO Jian, GONG Tongzhao, ZHANG Shaohua, ZHANG Jian |
| 图5 不同Cu含量K4061合金试样铸态组织的SEM像 |
| Fig.5 SEM images of as-cast K4061 (a), K4061-2Cu (b), K4061-5Cu (c), K4061-8Cu (d), and K4061-10Cu (e) alloys |
|