高温压缩变形Al-Zn-Mg-Cu合金动态再结晶后的{111}/{111}近奇异晶界 |
| 刘光辉, 王卫国, Rohrer Gregory S, 陈松, 林燕, 童芳, 冯小铮, 周邦新 |
|
{111}/{111} Near Singular Boundaries in a Dynamically Recrystallized Al-Zn-Mg-Cu Alloy Compressed at Elevated Temperature |
| LIU Guanghui, WANG Weiguo, Rohrer Gregory S, CHEN Song, LIN Yan, TONG Fang, FENG Xiaozheng, ZHOU Bangxin |
| 图14 铝合金压缩变形CDRX及DDRX面积分数随压缩应变速率的变化 |
| Fig.14 Area fractions of CDRX and DDRX versus compressing strain rate for Al alloys (Compressed at 520oC with true strain 1.2) |
|