高温压缩变形Al-Zn-Mg-Cu合金动态再结晶后的{111}/{111}近奇异晶界
刘光辉, 王卫国, Rohrer Gregory S, 陈松, 林燕, 童芳, 冯小铮, 周邦新

{111}/{111} Near Singular Boundaries in a Dynamically Recrystallized Al-Zn-Mg-Cu Alloy Compressed at Elevated Temperature
LIU Guanghui, WANG Weiguo, Rohrer Gregory S, CHEN Song, LIN Yan, TONG Fang, FENG Xiaozheng, ZHOU Bangxin
图12 A~C样品LAGB与HAGB中的{111}/{111}-NSB {111}重叠极图迹线分析
Fig.12 Overlapped {111} pole figure trace analyses for the {111}/{111}-NSBs from the LAGB and HAGB in samples A (a-d), B (e-h), and C (i-l)
(a, b) <11¯1¯>/5.7° (c, d) <11¯1¯>/48.4° (e, f) <1¯1¯1>/6.2°
(g, h) <111>/46.1° (i, j) <11¯1>/8.2° (k, l) <1¯11>/17.6°