高温压缩变形Al-Zn-Mg-Cu合金动态再结晶后的{111}/{111}近奇异晶界 |
| 刘光辉, 王卫国, Rohrer Gregory S, 陈松, 林燕, 童芳, 冯小铮, 周邦新 |
|
{111}/{111} Near Singular Boundaries in a Dynamically Recrystallized Al-Zn-Mg-Cu Alloy Compressed at Elevated Temperature |
| LIU Guanghui, WANG Weiguo, Rohrer Gregory S, CHEN Song, LIN Yan, TONG Fang, FENG Xiaozheng, ZHOU Bangxin |
| 图6 C样品中存在{111}/{111}-NSB的2组晶界的加权平均取向差Gauss分布曲线 |
| Fig.6 Weighted Gaussian misorientation distribution curves of two grain boundary groups containing {111}/{111}-NSBs in the sample C (FWHM—full width half maximum) (a) <111>/10° (b) <111>/45° |
|