高温压缩变形Al-Zn-Mg-Cu合金动态再结晶后的{111}/{111}近奇异晶界 |
| 刘光辉, 王卫国, Rohrer Gregory S, 陈松, 林燕, 童芳, 冯小铮, 周邦新 |
|
{111}/{111} Near Singular Boundaries in a Dynamically Recrystallized Al-Zn-Mg-Cu Alloy Compressed at Elevated Temperature |
| LIU Guanghui, WANG Weiguo, Rohrer Gregory S, CHEN Song, LIN Yan, TONG Fang, FENG Xiaozheng, ZHOU Bangxin |
| 图3 A~C样品具有特定旋转轴晶界的MD图 |
| Fig.3 MD maps of grain boundaries with specific rotation axis for the samples A-C (a) rotation around <001> (b) rotation around <011> (c) rotation around <012> (d) rotation around <013> (e) rotation around <111> (f) rotation around <112> (g) rotation around <113> (h) rotation around <122> |
|