冷却速率对锆合金氢化物析出的影响 |
| 公维佳, 梁森茂, 张敬翊, 李时磊, 孙勇, 李中奎, 李金山 |
|
Effect of Cooling Rate on Hydride Precipitation in Zirconium Alloys |
| GONG Weijia, LIANG Senmao, ZHANG Jingyi, LI Shilei, SUN Yong, LI Zhongkui, LI Jinshan |
| 图9 锆合金中氢化物与氢化物孪晶形成示意图 |