三方Cr5Te8 的磁结构和反常热膨胀 |
| 任卫军, 安萌, 高飞, 罗小华, 李昺, 张志东, 王进威 |
|
Magnetic Structure and Abnormal Thermal Expansion of Trigonal Cr5Te8 |
| REN Weijun, AN Meng, GAO Fei, LUO Xiaohua, LI Bing, ZHANG Zhidong, WANG Chin-Wei |
| 图5 Cr5Te8 3.3 K NPD谱及其精修结果,及Cr5Te8磁结构示意图 |
| Fig.5 Cr5Te8 NPD spectra at 3.3 K and the refinement (a), and schematic of the magnetic structure of Cr5Te8 (b) |
|