C包覆Ni磁性载体负载Pt催化硝基苯加氢性能 |
| 武逸, 司阳, 黄彦民, 刁江勇, 孟繁敬, 刘增, 刘洪阳 |
|
Hydrogenation of Nitrobenzene Catalyzed by Pt Supported on Carbon Coated Nickel Magnetic Supports |
| WU Yi, SI Yang, HUANG Yanmin, DIAO Jiangyong, MENG Fanjing, LIU Zeng, LIU Hongyang |
| 图5 0.1%Pt1/Ni@NG、0.3%Ptn/Ni@NG和0.5%Ptp/Ni@NG催化剂的高角环形暗场(HAADF) STEM像 |
| Fig.5 Low (a, c, e) and high (b, d, f) magnified HAADF STEM images of 0.1%Pt1/Ni@NG (a, b), 0.3%Ptn/Ni@NG (c, d), and 0.5%Ptp/Ni@NG (e, f) catalysts (White labels indicate Pt single atoms, blue labels indicate Pt nanoparticles, and red labels indicate Pt clusters) |
|