表3 (Y1/4Ho1/4Er1/4Yb1/4)2SiO5面层和Yb2SiO5面层Rietveld定量相分析结果及相应的精修因子
Table 3 Phase fractions in annealed (Y1/4Ho1/4Er1/4Yb1/4)2SiO5 and Yb2SiO5 topcoats and corresponding Rietveld refinements factors
CoatingPhase composition (mass fraction / %)Refinement factor / %
RE2SiO5RE2O3R-weighted pattern (Rwp)R-pattern (Rp)
(Y1/4Ho1/4Er1/4Yb1/4)2SiO576.323.74.943.65
Yb2SiO573.326.77.915.79