高熵稀土单硅酸盐环境障涂层局域结构的原子对分布函数解析
王浩宇, 吕熙睿, 陈琦, 熊瑛, 罗志新, 张洁, 王京阳

Neutron Pair Distribution Function Analysis to the Local Structure of High-Entropy RE2SiO5 Environmental Barrier Coating
WANG Haoyu, LÜ Xirui, CHEN Qi, XIONG Ying, LUO Zhixin, ZHANG Jie, WANG Jingyang
表2 EBC各层的Young's模量及热膨胀系数(CTE)[10,22,23,25~29]
Table 2 Young's moduli and coefficients of thermal expansion (CTE) of EBC system components[10,22,23,25-29]
LayerMaterialYoung's modulus / GPaCTE / (106 K-1)Ref.
SubstrateSiC4304.02[25]
Bond layerSi82*4.10[23]
Inter layerYb2Si2O772-85*4.66[22,26]
Yb2SiO570-80*6.5-7.32[27]
Top layerYb2O390.85*6.07-8.03[28]
(4RE1/4)2SiO572.5-85*5.49-6.59[10]