高熵稀土单硅酸盐环境障涂层局域结构的原子对分布函数解析 |
| 王浩宇, 吕熙睿, 陈琦, 熊瑛, 罗志新, 张洁, 王京阳 |
|
Neutron Pair Distribution Function Analysis to the Local Structure of High-Entropy RE2SiO5 Environmental Barrier Coating |
| WANG Haoyu, LÜ Xirui, CHEN Qi, XIONG Ying, LUO Zhixin, ZHANG Jie, WANG Jingyang |
| 图8 (Y1/4Ho1/4Er1/4Yb1/4)2SiO5和Yb2SiO5的PDF谱图PDFgui精修结果及拟合结构的原子对分析 |
| Fig.8 PDF Rietveld refinement patterns of (Y1/4Ho1/4Er1/4-Yb1/4)2SiO5 (a) and Yb2SiO5 (b), and corresponding derived partial PDFs |
|