高熵稀土单硅酸盐环境障涂层局域结构的原子对分布函数解析 |
| 王浩宇, 吕熙睿, 陈琦, 熊瑛, 罗志新, 张洁, 王京阳 |
|
Neutron Pair Distribution Function Analysis to the Local Structure of High-Entropy RE2SiO5 Environmental Barrier Coating |
| WANG Haoyu, LÜ Xirui, CHEN Qi, XIONG Ying, LUO Zhixin, ZHANG Jie, WANG Jingyang |
| 图7 采用Rietveld精修TOF-NPD数据获得的RE2SiO5晶体结构直接拟合PDF的拟合结果 |
| Fig.7 Fit of RE2SiO5 PDF with structures obtained from the TOF-NPD Rietveld refinements (G(r) is defined as atomic pair distribution funtion, r—distance between atoms in the system) |
|