高熵稀土单硅酸盐环境障涂层局域结构的原子对分布函数解析 |
| 王浩宇, 吕熙睿, 陈琦, 熊瑛, 罗志新, 张洁, 王京阳 |
|
Neutron Pair Distribution Function Analysis to the Local Structure of High-Entropy RE2SiO5 Environmental Barrier Coating |
| WANG Haoyu, LÜ Xirui, CHEN Qi, XIONG Ying, LUO Zhixin, ZHANG Jie, WANG Jingyang |
| 图3 (Y1/4Ho1/4Er1/4Yb1/4)2SiO5/Yb2Si2O7/Si和Yb2SiO5/Yb2Si2O7/Si涂层退火态与热循环后的SEM整体截面形貌及纵向裂纹放大形貌 |
| Fig.3 Cross-section SEM images of (Y1/4Ho1/4Er1/4Yb1/4)2SiO5/Yb2Si2O7/Si (a, c, e, f) and Yb2SiO5/Yb2Si2O7/Si (b, d, g, h) coatings after annealing (a, b) and thermal cycling for 300 cyc (c, e, f) and 83 cyc (d, g, h) (White arrows in Fig.2c indicate the locations of vertical cracks in top layer) |
|