高熵稀土单硅酸盐环境障涂层局域结构的原子对分布函数解析
王浩宇, 吕熙睿, 陈琦, 熊瑛, 罗志新, 张洁, 王京阳

Neutron Pair Distribution Function Analysis to the Local Structure of High-Entropy RE2SiO5 Environmental Barrier Coating
WANG Haoyu, LÜ Xirui, CHEN Qi, XIONG Ying, LUO Zhixin, ZHANG Jie, WANG Jingyang
图2 (Y1/4Ho1/4Er1/4Yb1/4)2SiO5/Yb2Si2O7/Si和Yb2SiO5/Yb2Si2O7/Si涂层退火态XRD谱
Fig.2 XRD spectra of (Y1/4Ho1/4Er1/4Yb1/4)2SiO5/Yb2-Si2O7/Si (a) and Yb2SiO5/Yb2Si2O7/Si (b) coatings after annealing