高熵稀土单硅酸盐环境障涂层局域结构的原子对分布函数解析 |
| 王浩宇, 吕熙睿, 陈琦, 熊瑛, 罗志新, 张洁, 王京阳 |
|
Neutron Pair Distribution Function Analysis to the Local Structure of High-Entropy RE2SiO5 Environmental Barrier Coating |
| WANG Haoyu, LÜ Xirui, CHEN Qi, XIONG Ying, LUO Zhixin, ZHANG Jie, WANG Jingyang |
| 图1 三层结构环境障涂层(EBC)的SEM像及有限元网格模型 |
| Fig.1 Cross-sectional SEM image and finite element mesh model of tri-layer structured environmental barrier coating (EBC) |
|