Pd-Si金属玻璃液-液相变过程的短程-中程序结构演变规律
董蔚霞, 姚忠正, 刘思楠, 陈国星, 王循理, 吴桢舵, 兰司

Evolution of Short-to-Medium Range Orders During the Liquid-Liquid Phase Transition of a Pd-Si Metallic Glass
DONG Weixia, YAO Zhongzheng, LIU Sinan, CHEN Guoxing, WANG Xun-Li, WU Zhenduo, LAN Si
表1 约化对分布函数中不同峰的积分强度在结晶前后的变化趋势
Table 1 Summary of atomic pairs for different peaks in reduced pair distribution function patterns
Peak

Position

nm

Cluster structuret ≤ 200 st > 200 s
r10.278F + T↓↑
r210.406F + T▁↑
r220.486F + T↓↑
r230.547T↓↓
r310.638F↑↓
r320.702T↓↓
r330.742F + T▁↑
r340.846F▁↑
r410.938T↓↓
r420.101F↑↑