Pd-Si金属玻璃液-液相变过程的短程-中程序结构演变规律 |
| 董蔚霞, 姚忠正, 刘思楠, 陈国星, 王循理, 吴桢舵, 兰司 |
|
Evolution of Short-to-Medium Range Orders During the Liquid-Liquid Phase Transition of a Pd-Si Metallic Glass |
| DONG Weixia, YAO Zhongzheng, LIU Sinan, CHEN Guoxing, WANG Xun-Li, WU Zhenduo, LAN Si |
| 图6 约化对分布函数G(r)上属于晶体结构的特征峰(即随着结晶过程新产生的特征原子对)的积分强度演变图 |
| Fig.6 Integrated intensity of atomic pairs in the newly formed crystalline peaks of r21 (a), r31 (b), r33 (c), and r42 (d) (Insets show the enlarged views of integrated intensity of corresponding atomic pairs at the beginning of isothermal annealing. Arrows indicate the trend of integrated intensity before crystallization) |
|