Pd-Si金属玻璃液-液相变过程的短程-中程序结构演变规律 |
| 董蔚霞, 姚忠正, 刘思楠, 陈国星, 王循理, 吴桢舵, 兰司 |
|
Evolution of Short-to-Medium Range Orders During the Liquid-Liquid Phase Transition of a Pd-Si Metallic Glass |
| DONG Weixia, YAO Zhongzheng, LIU Sinan, CHEN Guoxing, WANG Xun-Li, WU Zhenduo, LAN Si |
| 图5 约化对分布函数G(r)上属于非晶结构的特征峰(即退火前超过冷液体中已经存在的特征原子对)的积分强度演变图 |
| Fig.5 Integrated intensity of atomic pairs in the original amorphous phase peaks of r1 (a), r22 (b), r23 (c), and r32 (d) (Insets show the enlarged views of integrated intensity of corresponding atomic pairs at the beginning of isothermal annealing. Arrows indicate the trends of integrated intensity before crystallization) |
|