Pd-Si金属玻璃液-液相变过程的短程-中程序结构演变规律 |
| 董蔚霞, 姚忠正, 刘思楠, 陈国星, 王循理, 吴桢舵, 兰司 |
|
Evolution of Short-to-Medium Range Orders During the Liquid-Liquid Phase Transition of a Pd-Si Metallic Glass |
| DONG Weixia, YAO Zhongzheng, LIU Sinan, CHEN Guoxing, WANG Xun-Li, WU Zhenduo, LAN Si |
| 图3 Pd82Si18金属玻璃在超过冷液相区等温退火过程中第一衍射峰Q1峰位与峰宽演变图 |
| Fig.3 Evolution of peak position (a) and peak width (b) of the 1st diffraction peak Q1 during the isothermal annealing for Pd82Si18 metallic glass (Insets show the enlarged views of peak position and peak width at the beginning of isothermal annealing. Arrows show the trends of the peak position and peak width before crystallization) |
|