Pd-Si金属玻璃液-液相变过程的短程-中程序结构演变规律 |
| 董蔚霞, 姚忠正, 刘思楠, 陈国星, 王循理, 吴桢舵, 兰司 |
|
Evolution of Short-to-Medium Range Orders During the Liquid-Liquid Phase Transition of a Pd-Si Metallic Glass |
| DONG Weixia, YAO Zhongzheng, LIU Sinan, CHEN Guoxing, WANG Xun-Li, WU Zhenduo, LAN Si |
| 图2 Pd82Si18金属玻璃在超过冷液相区等温退火过程,S(Q)曲线上不同结晶峰积分强度的演变分析图 |
| Fig.2 Analyses of the integrated intensity of crystalline peaks Q12 (a), Q21 (b), Q22 (c), and Q23 (d) in S(Q)during the isothermal annealing for Pd82Si18 metallic glass (Insets show the enlarged views of integrated intensity at the beginning of isothermal annealing. The arrow in inset of Fig.2a marks the time when crystallization begins. t—isothermal annealing time) |
|