利用小角中子核磁散射分离研究AerMet100钢中纳米析出相的形貌和成分
柯于斌, 李彬, 段辉平

Morphology and Chemical Composition of Nanoprecipitate in AerMet100 Steel by Separation of the Nuclear and Magnetic Small-Angle Neutron Scattering Data
KE Yubin, LI Bin, DUAN Huiping
表3 AerMet100钢SANS磁散射拟合结果 (nm)
Table 3 Fitted structural parameters of nanodomains from the magnetic SANS data of AerMet100 steel
SampleDLRHSt
CoNi_4541.80 ± 0.746.51 ± 0.425.01 ± 0.470
CoNi_4822.46 ± 0.7513.70 ± 1.2418.50 ± 0.412.59 ± 0.47
CoNi_4862.60 ± 0.8613.40 ± 1.5018.00 ± 0.355.56 ± 1.60
CoNi_4982.62 ± 0.4019.07 ± 1.6118.57 ± 0.465.57 ± 1.56