利用小角中子核磁散射分离研究AerMet100钢中纳米析出相的形貌和成分 |
| 柯于斌, 李彬, 段辉平 |
|
Morphology and Chemical Composition of Nanoprecipitate in AerMet100 Steel by Separation of the Nuclear and Magnetic Small-Angle Neutron Scattering Data |
| KE Yubin, LI Bin, DUAN Huiping |
| 图1 CoNi_454样品透过率曲线的Bragg边,及沿0°和90°方向按10°角进行积分和规约 |
| Fig.1 Transmission curve and Bragg-edge feature of CoNi_454 sample (a), integration and normalization within 10° azimuth angle along the 0° and 90° orientations (b) (Qx, Qy —scattering vector moduli in x and y axes, repectively) |
|