退火热处理对增材制造AlSi10Mg合金宏观和微观变形行为的影响 |
| 张星星, LUTZ Andreas, 甘为民, MAAWAD Emad, KRIELE Armin |
|
Effect of Annealing Heat Treatment on the Macroscopic and Microscopic Deformation Behavior of Additively Manufactured AlSi10Mg Alloy |
| ZHANG Xingxing, LUTZ Andreas, GAN Weimin, MAAWAD Emad, KRIELE Armin |
| 图7 Al和Si两相对合金加工硬化率的贡献(这里重新绘制了图2b中的合金数据用于对比) |
| Fig.7 Contributions of Al and Si phases to the strain hardening rate of the alloys (The data of alloys in Fig.2b was plotted here again for comparison) (a) as-built sample (b) annealed sample |
|