退火热处理对增材制造AlSi10Mg合金宏观和微观变形行为的影响 |
| 张星星, LUTZ Andreas, 甘为民, MAAWAD Emad, KRIELE Armin |
|
Effect of Annealing Heat Treatment on the Macroscopic and Microscopic Deformation Behavior of Additively Manufactured AlSi10Mg Alloy |
| ZHANG Xingxing, LUTZ Andreas, GAN Weimin, MAAWAD Emad, KRIELE Armin |
| 图2 打印态和退火态试样的宏观力学行为 |
| Fig.2 Macroscopic behaviors of as-built and annealed samples (a) engineering stress-strain curves (b) hardening coefficient curves (c) determination of uniform true strain |
|