稀土元素Ce对挤压态Mg-0.3Al-0.2Ca-0.5Mn合金板材体织构及力学各向异性的影响 |
||||||||||||||||
| 朱桂杰, 王思清, 查敏, 李眉娟, 孙凯, 陈东风 | ||||||||||||||||
|
Effect of Rare Earth Element Ce on the Bulk Texture and Mechanical Anisotropy of As-Extruded Mg-0.3Al- 0.2Ca-0.5Mn Alloy Sheets |
||||||||||||||||
| ZHU Guijie, WANG Siqing, ZHA Min, LI Meijuan, SUN Kai, CHEN Dongfeng | ||||||||||||||||
| 表3 AXM、AXM + 0.05Ce和AXM + 0.5Ce合金的轴比c / a |
||||||||||||||||
| Table 3 c / a values obtained by the XRD data of the AXM, AXM + 0.05Ce, and AXM + 0.5Ce alloys |
||||||||||||||||
|
||||||||||||||||