稀土元素Ce对挤压态Mg-0.3Al-0.2Ca-0.5Mn合金板材体织构及力学各向异性的影响
朱桂杰, 王思清, 查敏, 李眉娟, 孙凯, 陈东风

Effect of Rare Earth Element Ce on the Bulk Texture and Mechanical Anisotropy of As-Extruded Mg-0.3Al- 0.2Ca-0.5Mn Alloy Sheets
ZHU Guijie, WANG Siqing, ZHA Min, LI Meijuan, SUN Kai, CHEN Dongfeng
图9 挤压态AXM、AXM + 0.05Ce和AXM + 0.5Ce合金板材沿着ED和TD的(0001)<112¯0>基面滑移Schmid因子(SF)分布图
Fig.9 Schmid factor (SF) distribution maps of (0001)<112¯0> basal slip of the as-extruded AXM (a, b), AXM + 0.05Ce (c, d), and AXM + 0.5Ce (e, f) alloy sheets along ED (a, c, e) and TD (b, d, f)