稀土元素Ce对挤压态Mg-0.3Al-0.2Ca-0.5Mn合金板材体织构及力学各向异性的影响 |
| 朱桂杰, 王思清, 查敏, 李眉娟, 孙凯, 陈东风 |
|
Effect of Rare Earth Element Ce on the Bulk Texture and Mechanical Anisotropy of As-Extruded Mg-0.3Al- 0.2Ca-0.5Mn Alloy Sheets |
| ZHU Guijie, WANG Siqing, ZHA Min, LI Meijuan, SUN Kai, CHEN Dongfeng |
| 图6 挤压态AXM、AXM + 0.05Ce和AXM + 0.5Ce合金板材沿横向(TD)和挤压方向(ED)的室温拉伸力学性能及TD和ED方向拉伸屈服强度比 |
| Fig.6 Mechanical properties at room temperature of the as-extruded AXM (a), AXM + 0.05Ce (b), and AXM + 0.5Ce (c) alloy sheets along ED and TD; and tensile yield strength (TYS) ratio along ED and TD (d) |
|