稀土元素Ce对挤压态Mg-0.3Al-0.2Ca-0.5Mn合金板材体织构及力学各向异性的影响 |
| 朱桂杰, 王思清, 查敏, 李眉娟, 孙凯, 陈东风 |
|
Effect of Rare Earth Element Ce on the Bulk Texture and Mechanical Anisotropy of As-Extruded Mg-0.3Al- 0.2Ca-0.5Mn Alloy Sheets |
| ZHU Guijie, WANG Siqing, ZHA Min, LI Meijuan, SUN Kai, CHEN Dongfeng |
| 图4 挤压态AXM、AXM + 0.05Ce和AXM + 0.5Ce合金板材的高倍SEM-BSE像和EDS分析 |
| Fig.4 High magnification SEM-BSE images (a-c) and EDS analyses (d-f) of the as-extruded AXM (a, d), AXM + 0.05Ce (b, e), and AXM + 0.5Ce (c, f) alloy sheets, where Figs.4d-f are line-scan results of the typical second-phase particle at square regions A, B, and C in Figs.4a-c, respectively |
|