稀土元素Ce对挤压态Mg-0.3Al-0.2Ca-0.5Mn合金板材体织构及力学各向异性的影响
朱桂杰, 王思清, 查敏, 李眉娟, 孙凯, 陈东风

Effect of Rare Earth Element Ce on the Bulk Texture and Mechanical Anisotropy of As-Extruded Mg-0.3Al- 0.2Ca-0.5Mn Alloy Sheets
ZHU Guijie, WANG Siqing, ZHA Min, LI Meijuan, SUN Kai, CHEN Dongfeng
图3 挤压态AXM、AXM + 0.05Ce和AXM + 0.5Ce合金板材的XRD谱
Fig.3 XRD spectra of the as-extruded AXM, AXM + 0.05Ce, and AXM + 0.5Ce alloy sheets (a), and partially enlarged XRD spectra (b)