稀土元素Ce对挤压态Mg-0.3Al-0.2Ca-0.5Mn合金板材体织构及力学各向异性的影响 |
| 朱桂杰, 王思清, 查敏, 李眉娟, 孙凯, 陈东风 |
|
Effect of Rare Earth Element Ce on the Bulk Texture and Mechanical Anisotropy of As-Extruded Mg-0.3Al- 0.2Ca-0.5Mn Alloy Sheets |
| ZHU Guijie, WANG Siqing, ZHA Min, LI Meijuan, SUN Kai, CHEN Dongfeng |
| 图1 挤压态AXM、AXM + 0.05Ce和AXM + 0.5Ce合金板材显微组织的EBSD像和晶粒尺寸分布图 |
| Fig.1 EBSD images (a, c, e) and grain size distributions (b, d, f) of the as-extruded AXM (a, b), AXM + 0.05Ce (c, d), and AXM + 0.5Ce (e, f) alloy sheets (dave—average grain size) |
|