焊前预处理对钛合金厚板焊接残余应力的影响 |
| 周牧, 王倩, 王延绪, 翟梓融, 何伦华, 李昺, 马英杰, 雷家峰, 杨锐 |
|
Effect of Prewelding Pretreatment on Welding Residual Stress of Titanium Alloy Thick Plate |
| ZHOU Mu, WANG Qian, WANG Yanxu, ZHAI Zirong, HE Lunhua, LI Bing, MA Yingjie, LEI Jiafeng, YANG Rui |
| 图7 ND法无应力样品不同探测器(D1、D2) 4 h的检测曲线和(101) α 晶面间距拟合结果 |
| Fig.7 ND method data of stress-free samples by different detectors (D1, D2) at 4 h (a) and (101) αd-spacing fitting results (b) (d-spacing—interplanar spacing) |
|