焊前预处理对钛合金厚板焊接残余应力的影响 |
| 周牧, 王倩, 王延绪, 翟梓融, 何伦华, 李昺, 马英杰, 雷家峰, 杨锐 |
|
Effect of Prewelding Pretreatment on Welding Residual Stress of Titanium Alloy Thick Plate |
| ZHOU Mu, WANG Qian, WANG Yanxu, ZHAI Zirong, HE Lunhua, LI Bing, MA Yingjie, LEI Jiafeng, YANG Rui |
| 图5 未预热和预热钛合金焊接接头距熔合线不同距离处热影响区(HAZ)的SEM像 |
| Fig.5 SEM images of HAZ at different distances from the fusion line of unpreheated (a-c) and preheated (d-h) titanium alloy welded joint (Insets show the corresponding high magnified images) (a) 0 mm (Near-FZ) (b) 2 mm (Mid-HAZ) (c) 4 mm (Near-BM) (d) 0 mm (Near-FZ) (e) 2 mm (Near-FZ) (f) 4 mm (Near-FZ) (g) 5 mm (Mid-HAZ) (h) 8 mm (Near-BM) |
|