焊前预处理对钛合金厚板焊接残余应力的影响 |
| 周牧, 王倩, 王延绪, 翟梓融, 何伦华, 李昺, 马英杰, 雷家峰, 杨锐 |
|
Effect of Prewelding Pretreatment on Welding Residual Stress of Titanium Alloy Thick Plate |
| ZHOU Mu, WANG Qian, WANG Yanxu, ZHAI Zirong, HE Lunhua, LI Bing, MA Yingjie, LEI Jiafeng, YANG Rui |
| 图3 未预热和预热钛合金焊接接头的OM像 |